Refractory mortar: for joints in corundum refractory masonry
Release time:2021-11-23 09:15:56    Author:

  Product Name: Zirconia Powder ZrO29

  Chemical composition content (wt%):

  Zirconia ZrO2: 99.30

       Alumina Al2O3: 0.30

       Silicon oxide SiO2: 0.20

       Titanium oxide TiO2: 0.15

       Iron oxide Fe2O3: 0:05

  Powder physical properties Micro: uniform spherical crystals

  color: White

  Processing method: using imported zircon sand as raw material, calcining, ball milling and spray drying

  Product features: The spray drying process is short, the ceramic powder product prepared by this method has high purity, low thermal conductivity, and the prepared coating has good heat insulation effect;

  Production method: laser cladding technology, plasma spraying, explosive spraying, supersonic flame spraying;

  The chain plate production line equipment is easy to clean, and the line body can directly wash the surface of the equipment with water (but it should be noted that the power part and the control part cannot be washed with water, so as to avoid damage to the internal parts, electric shock, and accidents). In order to make the service life of the equipment reach its value, maintenance and maintenance are the key. Generally speaking, the motor of the power part needs to be replaced in time after a year of use to ensure that the motor is in operation and reduce internal losses. Usually, after the chain plate production line equipment is used up, the power supply should be turned off in time, and the surface of the equipment should be cleaned for a period of time. When the equipment needs to be maintained, it should be maintained by experienced equipment personnel, and non-related personnel should not do it, so as to avoid unnecessary economic losses and safety accidents. When the equipment fails, do not blindly check and repair the chain plate as the bearing surface.