Bubble alumina brick

 

   · Introduction

 

Characteristics:Alumina bubble bricks use the hollow alumina sphere(bubble alumina), corundum powder, calcined powder as raw material, and are made through Homogenization, molding, high temperature sintering. High temperature resistance, low thermal conductivity, good thermal insulation, good chemical stability (acid-base erosion resistance), low bulk density (lighter than the same kind of material, thin kiln wall, low cost).

Application:Widely used in inner linings of various non-contacted melt high temperature kiln and thermal insulating layers of high temperature kilns.

 

   · Physical and chemical indicators

 

Name

MLQ84

MLQ90

LQ-1.2

LQ-1.5

LQ-1.7

LQ-2.0

Al2O3%≥

84

90

98.5

98.5

98.5

98.5

Fe2O3%≤

0.8

0.5

0.3

0.3

0.3

0.3

SiO2%≤

15

9

1.0

1.0

1.0

1.0

Bulk Density

g/cm3

1.5

1.5

1.2

1.5

1.7

2

Compressive Strength at Normal Temperature

MPa≥

16

15

13

12

15

20-25

Porosity %≥

58

60

62

60

58

52

Soften Point at 0.1MPa Load

℃ 0.1MPa≥

1650

1700

1700

1700

1700

1700

Refractoriness ℃≥

1800

1800

1800

1800

1800

1800

Thermal Conductivity

W/m·K(1000℃)≤

1.2

1.15

0.95

1.05

1.15

1.2